                Elimination of extraordinarily high cracking susceptibility of aluminum alloy fabricated by laser powder bed fusion
            文献摘要:
                    Using the calculation of phase diagrams approach and Scheil solidification modeling,the Al-2.5Mg-1.0Ni-0.4Sc-0.1Zr alloy was designed,intentionally with an extraordinarily high cracking susceptibility,making it prime for solidification cracking during laser powder bed fusion.This study demonstrates the abil-ity to mitigate even the most extreme solidification cracking tendencies in aluminum alloys with only minor alloying additions of Sc and Zr,0.5 wt.%max.Furthermore,by employing a simple direct ageing heat treatment,good tensile mechanical properties were observed with a yield strength of 308 MPa,an ultimate tensile strength of 390 MPa,and a total elongation of 11%.
                文献关键词:
                    
                中图分类号:
                    作者姓名:
                    
                        Holden Hyer;Le Zhou;Sharon Park;Thinh Huynh;Abhishek Mehta;Saket Thapliyal;Rajiv S.Mishra;Yongho Sohn
                    
                作者机构:
                    Department of Materials Science and Engineering,University of Central Florida,Orlando,FL,USA;Now Research Scientist,Oak Ridge National Laboratory,Oak Ridge,TN,USA;Now Assistant Professor,Marquette University,Milwaukee,WI,USA;Now PhD Candidate,Johns Hopkins University,Baltimore,MD,USA;Center for Friction Stir Processing,Department of Materials Science and Engineering,Advanced Materials and Manufacturing Processes Institute,University of North Texas,Denton,TX,USA
                文献出处:
                    
                引用格式:
                    
                        [1]Holden Hyer;Le Zhou;Sharon Park;Thinh Huynh;Abhishek Mehta;Saket Thapliyal;Rajiv S.Mishra;Yongho Sohn-.Elimination of extraordinarily high cracking susceptibility of aluminum alloy fabricated by laser powder bed fusion)[J].材料科学技术(英文版),2022(08):50-58
                    
                A类:
                4Sc
                B类:
                    Elimination,extraordinarily,high,cracking,susceptibility,aluminum,fabricated,by,laser,powder,bed,fusion,Using,calculation,phase,diagrams,approach,Scheil,solidification,modeling,5Mg,0Ni,1Zr,was,designed,intentionally,making,prime,during,This,study,demonstrates,abil,mitigate,even,most,extreme,tendencies,alloys,only,minor,alloying,additions,wt,max,Furthermore,employing,simple,direct,ageing,heat,treatment,good,tensile,mechanical,properties,were,observed,yield,strength,ultimate,total,elongation
                AB值:
                    0.645083
                相似文献
                
            机标中图分类号,由域田数据科技根据网络公开资料自动分析生成,仅供学习研究参考。