The fatigue crack behavior of U75V rail under different quenching rates was studied using SEM and CLSM. The results show that the pearlite interlayer spacing and fatigue crack growth rate decrease, and the deflection path of cracks and the number of branching cracks of U75V rail increases with an increase of cooling rate. The tearing edge of unstable region transites from pearlite lamellae to dimple. The fatigue crack growth path is closely related to the orientation of lamellae in pearlite microstructure. There are three modes direction of fatigue crack growth path and pearlite lamellar, which are parallel, vertical and 45° angle, and most of the branch cracks occur at an angle of 45 ° between the lamellar direction and the crack direction. More specifically, the deflection paths of cracks and branching crack have a relaxation effect on the stress intensity at the crack tip, which restrains the fatigue crack growth rate.
文献关键词:
作者姓名:
CEN Yaodong;CHEN Lin;JI Chunjiao;WANG Huijun;BAO Xirong
作者机构:
School of Materials and Metallurgy,Inner Mongolia University of Science and Technology,Baotou 014010,China
引用格式:
[1]CEN Yaodong;CHEN Lin;JI Chunjiao;WANG Huijun;BAO Xirong-.Fatigue Crack Growth Behavior of Eutectoid Steel Rail)[J].武汉理工大学学报(材料科学版)(英文版),2022(03):507-512
A类:
Eutectoid,transites
B类:
Fatigue,Crack,Growth,Behavior,Steel,Rail,fatigue,behavior,U75V,rail,under,different,quenching,rates,was,studied,using,CLSM,results,show,that,pearlite,interlayer,spacing,growth,decrease,deflection,cracks,number,branching,increases,cooling,tearing,edge,unstable,region,from,lamellae,dimple,is,closely,related,orientation,microstructure,There,are,three,modes,direction,lamellar,which,parallel,vertical,angle,most,occur,between,More,specifically,paths,have,relaxation,effect,stress,intensity,tip,restrains
AB值:
0.505641
相似文献
In situ Observation of Li Deposition-Induced Cracking in Garnet Solid Electrolytes
Jun Zhao;Yongfu Tang;Qiushi Dai;Congcong Du;Yin Zhang;Dingchuan Xue;Tianwu Chen;Jingzhao Chen;Bo Wang;Jingming Yao;Ning Zhao;Yanshuai Li;Shuman Xia;Xiangxin Guo;Stephen J.Harris;Liqiang Zhang;Sulin Zhang;Ting Zhu;Jianyu Huang-Clean Nano Energy Center,State Key Laboratory of Metastable Materials Science and Technology,Yanshan University,Qinhuangdao 066004,China;Hebei Key Laboratory of Applied Chemistry,School of Environmental and Chemical Engineering,Yanshan University,Qinhuangdao 066004,China;Woodruff School of Mechanical Engineering,Georgia Institute of Technology,Atlanta Georgia 30332,USA;Department of Engineering Science and Mechanics,The Pennsylvania State University,University Park PA 16802,USA;College of Physics,Qingdao University,Qingdao 266071,China;Energy Storage Division,Lawrence Berkeley,National Laboratory,Berkeley CA 94720,USA;School of Materials Science and Engineering,Xiangtan University,Xiangtan 411105,China
机标中图分类号,由域田数据科技根据网络公开资料自动分析生成,仅供学习研究参考。