Effect of Al addition and heat treatment on the microstructures and corrosion resistance of Mg-Cu alloys
文献摘要:
The effects of Al content and annealing condition on the microstructures and corrosion performances of Mg-3 wt.%Cu-xAl(x=0,4 wt.%,8 wt.%)alloys were investigated.The Mg-3 wt.%Cu alloy contains Mg2Cu phase,but Al-bearing alloys contain MgAlCu and Mg17Al12 phases.The Mg2Cu and MgAlCu phases exhibit much higher Volta potential compared to Mg17Al12 and α-Mg,and their volume fractions are related to Al content of alloys and annealing condition.The weight loss measurement and electrochemical tests are conducted to explore the corrosion performances of alloys.The close relationship between weight loss rate of alloys and volume fraction of Cu-bearing phases indicates that the corrosion performances of alloys can be controlled by adjusting Al content of alloys and annealing conditions.
文献关键词:
作者姓名:
X.W.Wang;W.Wang;W.Chen;D.M.Chen
作者机构:
Shi-changxu Innovation Center for Advanced Materials,Institute of Metal Research,Chinese Academy of Sciences,Shenyang 110016,China;College of Material Science and Engineering,University of Science and Technology of China,Shenyang 110016,China
引用格式:
[1]X.W.Wang;W.Wang;W.Chen;D.M.Chen-.Effect of Al addition and heat treatment on the microstructures and corrosion resistance of Mg-Cu alloys)[J].材料科学技术(英文版),2022(03):219-232
A类:
B类:
Effect,addition,heat,treatment,microstructures,corrosion,resistance,alloys,effects,content,annealing,performances,wt,xAl,were,investigated,contains,Mg2Cu,but,bearing,MgAlCu,Mg17Al12,phases,exhibit,much,higher,Volta,potential,compared,their,volume,fractions,related,weight,loss,measurement,electrochemical,tests,conducted,explore,close,relationship,between,rate,indicates,that,can,controlled,by,adjusting,conditions
AB值:
0.442562
相似文献
Influence of Zr and Mn additions on microstructure and properties of Mg–2.5wt%Cu–Xwt%Zn (X = 2.5, 5 and 6.5) alloys
A.V.Koltygin;V.E.Bazhenov;I.V.Plisetskaya;V.A.Bautin;A.I.Bazlov;N.Y.Tabachkova;O.O.Voropaeva;A.A.Komissarov;V.D.Belov-Foundry Department,National University of Science and Technology(MISiS),Moscow 119049,Russia;Department of Metallurgy Steel,New Production Technologies and Protection of Metals,National University of Science and Technology(MISiS),Moscow119049,Russia;Laboratory of Advanced Green Materials,National University of Science and Technology(MISiS),Moscow 119049,Russia;Department of Materials Science of Semiconductors and Dielectrics,National University of Science and Technology(MISiS),Moscow 119049,Russia;Fianit Laboratory(Laser Materials and Technology Research Center at GPI),Prokhorov General Physics Institute RAS,Moscow 119991,Russia;Laboratory of Hybrid Nanostructured Materials,National University of Science and Technology(MISiS),Moscow 119049,Russia;Laboratory of Medical Bioresorption and Bioresistance,Moscow State University of Medicine and Dentistry,Moscow 127473,Russia
机标中图分类号,由域田数据科技根据网络公开资料自动分析生成,仅供学习研究参考。